Product name: E92 Bronze wrapped Bushing
-
-
Price: ASK
-
-
Post date: 2016-12-19
-
-
Stock Quantity: 1000
-
Description:
E90F/E92 14090, E90F/E92 14095, E90F/E92 140100, E90F/E92 14560, E90F/E92 14570, E90F/E92 14580, E90F/E92 14590, E90F/E92 145100, E90F/E92 15060, E90F/E92 15070, E90F/E92 15080, E90F/E92 15090, E90F/E92 150100, E90F/E92 15560, E90F/E92 15570, E90F/E92 15580, E90F/E92 15590, E90F/E92 155100, E90F/E92 16060, E90F/E92 16070, E90F/E92 16080, E90F/E92 16090, E90F/E92 160100, E90F/E92 16560, E90F/E92 16570, E90F/E92 16580, E90F/E92 16590, E90F/E92 165100, E90F/E92 17060, E90F/E92 17070, E90F/E92 17080, E90F/E92 17090, E90F/E92 170100, E90F/E92 17560, E90F/E92 17570
E92 is deriving from E90; the difference between E90 & E92
is Indentations on working surface, which substituted by Through-holes. Theses
holes will allow greater capacity to collect lubricant, which build up a
lubrication film at the start of movement and reduce the frication. It is
suitable for high load, lower speed application like construction, Transport,
and agriculture machinery.
E92 Chemical Composition
Part No | Material | Cu | Sn | P | Pb | Zn |
E92 | CuSn8 | 91.3% | 8.5% | 0.2% | / | / |
E92 Material Characteristics
Max. Load Capacity | ||
Static Load | N/mm2 | 120 |
Dynamic Load | N/mm2 | 40 |
Max. Speed | ||
m/s | 2.0 | |
m/s | >2.5 | |
Max. PV Value | N/mm2· m/s | 2.8 |
Tensile Strength | N/mm2 · m/s | 450 |
Yiled Point | N/mm2 · m/s | 250 |
Hardness | HB | 90-120 |
Elongation | 40% | |
Coefficient of Friction | μ | 0.08~0.25 |
Operation Temperature Range | ℃ | -100~200 |
Thermal Conductivity | W/(m · k) | 60 |
Coefficient of Thermal Expansion | k-1 | 15×10-6 |
E92 Oil Indentations/Holes
Corresponding Symbol
Epen | GGB | KS/INA | Federal Mogul | Techymon | SKF | Daido |
E92 | LD | Deva eco 7 | BRM-80 |